'''Recommendation'''<br>
'''Recommendation'''<br>
Test your system annually to ensure the electrical systems are not causing anodes to be consumed at a fast rate.<br><br>
Test your system annually to ensure the electrical systems are not causing anodes to be consumed at a fast rate<br><br>


'''Resources'''<br>
'''Resources'''<br>
Presentation Marine Galvanic Corrosion Made Easy: [[File:Marine Galvanic Corrosion Made Easy.pdf|thumb|Link]]<br>
Presentation Marine Galvanic Corrosion Made Easy: [[File:Marine Galvanic Corrosion Made Easy.pdf|thumb|Link]]<br>
Testing procedure: [https://www.strikhedonia.com/cathodic-testing-and-galvanic-isolation/ External Link]<br>
Cathodic testing procedure: [https://www.strikhedonia.com/cathodic-testing-and-galvanic-isolation/ External Link]<br>
Electrolysis Blocker Datasheet: [[File:Shore Power Electrolysis Blocker.pdf|thumb|Link]]<br>
Electrolysis Blocker Datasheet: [[File:Shore Power Electrolysis Blocker.pdf|thumb|Link]]<br>

Latest revision as of 13:22, 11 May 2026

Possible galvanic problems

Erosion of saildrive
Erosion of propellers
Erosion of rudder stock
Erosion of thru hulls
Prop-speed/saildrive paint flaking off
Bottom paint around thruhulls flaking off

Dangers

When zinc anodes are not replaced
When connected to shore power
When there are wiring issues on a sailboat

Best practices shore power

Have an isolation transformer installed OR
Have a electrolysis blocker installed

Recommendation
Test your system annually to ensure the electrical systems are not causing anodes to be consumed at a fast rate

Resources
Presentation Marine Galvanic Corrosion Made Easy: File:Marine Galvanic Corrosion Made Easy.pdf
Cathodic testing procedure: External Link
Electrolysis Blocker Datasheet: File:Shore Power Electrolysis Blocker.pdf